Causes Of Refractory Damage in Rotary Kilns - Chemical Damage

Jan 22, 2025

Leave a message

Several of the more common causes of chemical damage to resistant materials:

 

Alkali salt permeation / clinker liquid phase permeation

 

 In alkali-sulfur equilibrium, the alkali sulfur forms alkali salts and there is no excess alkali sulfur to thermochemically react with the refractory and chemically attack it. However, the alkali sulfur will still penetrate into the internal structure of the brick through the pores of the refractory brick, making the structure brittle and thus changing the performance of the refractory material.

 

 However, if the alkali sulphur is not balanced, not only will the alkali sulphur penetrate into the internal structure of the brick through the pores, but also the excess sulphur or potassium will react thermochemically with the refractory of different materials to form new low melting-point minerals or to form new minerals that will cause the volume of the refractory to expand.

 

2020121593236220080

 

 In addition, excessive alkali, chlorine, and sulfur are also causes of infiltration, when there is an excess of alkali or sulfur in the rotary kiln, this not only occurs with alkali salt infiltration, but also other damages, such as circling or crusting clogging.

 

20201215932514636035

 

 

Oxidation reduction

 

 Redox is one of the chemical damage phenomena, which is mainly caused by the lack of sufficient oxygen in the rotary kiln. Why is there a lack of oxygen in a rotary kiln? There are many reasons for this, including improper flame control, reasons for the operation of the coal injection pipe, and the use of uneven coal for combustion.

 

 When there is too much sulfur in the kiln gas, sulfate can easily penetrate the refractory bricks and form sulfides under strong reducing atmosphere conditions. Once the kiln conditions change from a reducing atmosphere to an oxidizing atmosphere, sulfide oxidation occurs, which leads to a significant increase in the volume of the refractory bricks and destroys the structure of the refractory bricks.

 

2020121593335256762

 

Hydration issues

 

 Since magnesium refractory bricks are extremely sensitive to water, rain, seawater or humid air can easily lead to hydration problems, thus destroying the structure of the refractory bricks.

 

 The most common reason is due to improper storage of refractory materials or damaged packaging, which leads to water penetration into the refractory bricks, causing chemical reactions, causing cracks on the surface of the bricks and destroying their structure, thus affecting the performance of the refractory bricks. Only the refractory bricks stored in a covered warehouse and keep the environment dry can effectively prevent the hydration problem.

 

The above situations are some common about the refractory material in the chemical aspects of the damage, therefore, we have to pay more attention to the operating conditions of the rotary kiln and refractory bricks in the use of the situation, in order to effectively prevent the premature destruction of refractory materials.