Oxygen blowing in steelmaking converters, oxygen enrichment in blast furnaces, oxygen enrichment in sintering, and oxygen cutting in the continuous casting process.

Oxygen plays a central role in several key aspects of steel production, and its application is closely integrated with the overall process. The following describes the processes of converter blowing in steelmaking, oxygen enrichment in the blast furnace, oxygen enrichment in sintering, and continuous casting and cutting, along with the specific roles of oxygen in each.
Steelmaking Converter Blowing (Oxygen Top-Blown Converter Steelmaking)
Core purpose: To oxidize impurities (carbon, silicon, manganese, phosphorus, etc.) in the molten iron using oxygen, and to refine the molten iron into steel.

Process Flow:
Charging: Load the converter with molten iron (70%–80%) and scrap (20%–30%). The molten iron serves as the main raw material, while the scrap helps regulate the temperature and recover resources.
1.Oxygen Blowing: High-pressure oxygen (purity ≥99.5%) is blown into the molten pool through the oxygen lance at the top of the converter (either immersed or semi-immersed). The oxygen pressure is typically 0.6–1.2 MPa, and the flow rate is adjusted according to the converter's capacity (e.g., approximately 20,000 m³/h for a 120-ton converter).
Oxygen first reacts with silicon and manganese in the molten iron (forming SiO₂ and MnO), releasing heat and rapidly raising the temperature of the molten pool (up to 1600–1700°C).
It then reacts with carbon to produce carbon monoxide gas (C + O₂ → CO↑). As the CO escapes from the molten pool, it stirs the melt, promoting a uniform reaction.
Phosphorus is oxidized to P₂O₅, which then reacts with lime (CaO) to form stable calcium phosphate (3CaO·P₂O₅) that enters the slag, achieving dephosphorization.
2.Slagging: During the oxygen blowing process, lime (CaO), fluorite (CaF₂), and other slagging agents are added to form an alkaline slag (mainly composed of CaO, SiO₂, MnO, etc.). The slag covers the surface of the molten steel, isolating it from the air to prevent secondary oxidation, while also absorbing impurities such as sulfur and phosphorus oxides.
3.End Point Control: The carbon content and temperature of the molten steel are measured using sub-lances or manual sampling. When the carbon content (e.g., ≤0.2% for mild steel) and temperature reach the target values, the oxygen blowing is stopped. The blowing time is usually between 10–20 minutes.
4.Steel Discharge: The converter is tilted to discharge the steel through the tap hole. At the same time, deoxidizers (such as ferrosilicon, ferromanganese, and aluminum) are added to remove residual oxygen, resulting in qualified steel.
Oxygen Enrichment in Blast Furnace (Oxygen-Enriched Blast in Blast Furnace Ironmaking)
Core purpose: To add oxygen to the blast air of the blast furnace, thereby increasing the oxygen concentration in the hot blast. This enhances coke combustion and the reduction reaction of iron ore, improving the overall efficiency of ironmaking.

Process Flow:
Raw Material Loading: Iron ore (sintered ore, pellet ore, etc.), coke (fuel and reducing agent), and limestone (slagging agent) are proportionally loaded in batches from the material bell or bell-less device at the top of the blast furnace to form a material column.
1.Oxygen-Enriched Blast: A mixture of hot air and oxygen is blown into the furnace shaft through the air outlet at the lower part of the blast furnace. (In a conventional blast, only hot air is used; in oxygen-enriched blast, pure oxygen is added to the hot air header via a pipeline.) This increases the oxygen concentration in the blast from the conventional 21% (air) to 23%–30%, adjusted according to the blast furnace's requirements.
·Oxygen reacts with coke (C + O₂ → CO₂↑ + heat; CO₂ + C → 2CO↑ + heat), releasing more heat and raising the furnace shaft temperature to 2000°C or higher.
·High-temperature CO acts as a reducing agent, reducing iron ore (such as Fe₂O₃) to iron (Fe₂O₃ + 3CO → 2Fe + 3CO₂↑). Oxygen enrichment accelerates the reduction reaction and shortens the residence time of iron ore in the furnace.
2.Separation of Slag and Iron: The liquid iron and slag (formed by impurities and slagging agents, with density less than iron) generated by the reduction process separate into layers in the furnace shaft. Iron is tapped from the iron outlet, and slag is removed through the slag outlet.
3.Gas Recovery: Blast furnace gas (mainly composed of CO, CO₂, and N₂) produced by the reaction is discharged from the top of the furnace and can be purified and recycled as fuel.
Effect of Oxygen Enrichment: Increasing the oxygen concentration by 1% can raise blast furnace output by 2%–3% and reduce coke consumption by approximately 1%.
Oxygen Enrichment in Sintering (Oxygen-Enriched Combustion in the Sintering Process)
Core purpose: To introduce oxygen during the sintering process of iron ore powder, enhance fuel combustion, and improve both the sintering speed and the quality of the sintered ore.

Process Flow:
Raw material preparation: Mix iron ore powder (60%–70%), fuel (coke powder or coal powder, 3%–5%), flux (limestone, dolomite, 10%–20%), and remineralization (sintering remineralization, 10%–20%), then add water to create a mixture with uniform particle size.
1.Fabrication and Ignition: The mixture is evenly spread on the sintering machine trolley to a thickness of about 300–500 mm. The surface fuel is ignited by the ignition furnace (using gas or natural gas combustion), with an ignition temperature of approximately 1100–1300°C. The sintering process is conducted at high temperature.
2.Oxygen-Enriched Extraction Sintering: After ignition, the extractor fan below the sintering machine draws air, causing the air (or oxygen-enriched air) to pass through the material layer from top to bottom. The fuel burns at a high temperature (1300–1500°C), causing minerals in the mixture (e.g., hematite, chalcopyrite) to soften, fuse, and bond, forming sinter lumps.
·Pure oxygen is added to the air extraction system, raising the oxygen concentration in the gas passing through the material layer to 23%–27%. This accelerates fuel combustion (with burning speed increasing by 30%–50%), expands the high-temperature sintering zone, and reduces fuel consumption by 5%–10%.
3.Cooling and Crushing: After sintering, the sintering trolley moves to the cooling section (blast or extraction cooling), reducing the temperature of the sintered ore from 800–1000°C to 100–200°C. The cooled sinter is then crushed and screened to a grain size of 10–50 mm (used as raw material for ironmaking in the blast furnace), and the screened fines are returned for re-sintering.
Effect of Oxygen Enrichment: Increasing the oxygen concentration by 1% can increase sinter output by 1.5%–2% and improve the strength of the sintered ore (reducing the powder rate).
Continuous Casting Cutting (Oxygen Cutting of Continuous Casting Billets)
Core purpose: To cut long billets from continuous casting into fixed lengths (e.g., 6–12 m) to facilitate subsequent rolling.

Process Flow:
Continuous casting into shape: The molten steel from the steel furnace is poured into the intermediate ladle of the continuous casting machine, and then evenly distributed to the crystallizer. In the crystallizer, the steel begins to solidify, forming a billet shell approximately 10–30 mm thick. The billet is then withdrawn from the crystallizer by a straightening machine and enters the secondary cooling zone (using water spray or mist cooling), where it completely solidifies (with no liquid phase remaining inside).
1.Cutting to Length: Fully solidified billets (including billets, slabs, round billets, etc.) are sent to the cutting area for oxygen cutting (flame cutting):
The cutting device (torch) emits a mixture of gas (e.g., acetylene, propane, natural gas) and oxygen, which ignites to generate a high temperature (approximately 3000°C), melting the metal on the surface of the billet.
Simultaneously, high-pressure cutting oxygen (purity ≥ 99.5%) is sprayed from the center of the torch, blowing away the molten metal (slag) and forming the cut. The relative movement between the torch and billet completes the cutting process.
2.Subsequent Processing: After cutting, the billet is inspected for surface quality and dimensional accuracy, then sent to the rolling shop for heating and rolling.
Role of Oxygen: Oxygen acts as a combustion agent to provide the high temperature necessary for gas combustion and simultaneously serves as the cutting oxygen to blow away slag, enabling rapid cutting. The cutting speed is adjusted according to billet thickness (for example, the cutting speed for a 200 mm thick slab is about 0.5–1 m/min).
Summary
Oxygen serves as both a "reinforcing agent" and an "oxidizing agent" in steel production: it oxidizes impurities to produce steel in the converter, accelerates reactions to improve efficiency in the blast furnace and sintering processes, and is used as a cutting medium to achieve precise cutting of continuous casting billets. Its application throughout the entire process-from ironmaking, sintering, steelmaking to continuous casting-is a core factor ensuring the efficient production of modern steel.